Repair of concrete concrete wall/ heightless part

This time, it is repair and color matching after cross- cross section repair .

It is not enough to meet the specified height, and the extra hit part is erased + face wood

The line was twisted, so I requested that it be arranged as a whole.

 

No, it was hot anyway ... (-_-;)

The sensible temperature exceeded 30 degrees Celsius!

What's so difficult is that the Repair Resin is a quick-drying repair material, so from the side you are kneading

It's getting hardened (; ´Д `)

Even if it is divided into a knead is knead , it will harden, so it will be impatient and impatient.

So knead it very softly.

 

When it's hot, knead the Repair Resin softly, and when it's cold, knead it a little harder.

The point is that it is easy to adjust according to the temperature at that time!

 

However, the heat is great for color matching!

If the spray and pattern dries quickly, you can save the trouble of using a heat gun or gas.

It's time saving + energy saving!

It ’s good, energy saving ♪

 

 

Before

 

 

 

 

← Additional parts

 

 

After

 

 

 

 

 

 

 

Before

 

 

 

 

← Additional parts

 

 

After

 

 

 

 

 

 

 

The line goes through and the finish is beautiful.

We are glad that the person in charge is very pleased!